TY - JOUR
T1 - Formation of Bi-Sr-Ca-Cu-O superconducting films by electrodeposition
AU - Martín-Gonzalez, María Soledad
AU - García-Jaca, Javier
AU - Morán, Emilio
AU - Alario-Franco, Miguel Ángel
PY - 1999/9
Y1 - 1999/9
N2 - Superconducting films of the Bi-Sr-Ca-Cu-O family of oxides were prepared by electrodeposition of the constituent metals followed by an oxidative thermal treatment. The influence of water, stirring of the electrolyte, cleaning of the substrate, and deposition time on the quality of the films were studied. Before the thermal treatment, the electrodeposited films consisted of a mixture of different metals and carbonates of the constituent elements. The oxidation of the metallic phases and the decomposition of the carbonates occurred in the ranges 260-280 °C and 400-470 °C, respectively. The final oxides were obtained after an oxidative thermal treatment at 800 °C. Lower temperatures were not sufficient for the preparation of the superconducting oxide films. The prepared Bi-2201 films consisted of a mixture of two phases with different strontium, bismuth, and oxygen contents. The Bi-2212 films were composed of platelike particles with a preference to orientate along the (001) direction. These films showed critical temperatures up to 92 K and critical current densities up to 15,000 A/cm2 (at 77 K and zero field) when the films were pressed before the thermal treatment.
AB - Superconducting films of the Bi-Sr-Ca-Cu-O family of oxides were prepared by electrodeposition of the constituent metals followed by an oxidative thermal treatment. The influence of water, stirring of the electrolyte, cleaning of the substrate, and deposition time on the quality of the films were studied. Before the thermal treatment, the electrodeposited films consisted of a mixture of different metals and carbonates of the constituent elements. The oxidation of the metallic phases and the decomposition of the carbonates occurred in the ranges 260-280 °C and 400-470 °C, respectively. The final oxides were obtained after an oxidative thermal treatment at 800 °C. Lower temperatures were not sufficient for the preparation of the superconducting oxide films. The prepared Bi-2201 films consisted of a mixture of two phases with different strontium, bismuth, and oxygen contents. The Bi-2212 films were composed of platelike particles with a preference to orientate along the (001) direction. These films showed critical temperatures up to 92 K and critical current densities up to 15,000 A/cm2 (at 77 K and zero field) when the films were pressed before the thermal treatment.
UR - https://www.scopus.com/pages/publications/0032595558
U2 - 10.1557/JMR.1999.0473
DO - 10.1557/JMR.1999.0473
M3 - Article
AN - SCOPUS:0032595558
SN - 0884-2914
VL - 14
SP - 3497
EP - 3505
JO - Journal of Materials Research
JF - Journal of Materials Research
IS - 9
ER -