Fragilizacion por hidrogeno de tubos de acero API 5LX-52 y X-60

Translated title of the contribution: Hydrogen embrittlement of API 5LX-52 and X-60 Pipe Line Steels

I. Azkarate*, E. Erauzkin, A. Pelayo, A. M. Irisarri

*Corresponding author for this work

    Research output: Contribution to journalArticlepeer-review

    Abstract

    The behavior of API 5LX-52 and X-60 pipe line steels was studied under two hydrogen embrittlement conditions, these were hydrogen embrittlement itself and hydrogen assisted stress cracking. Determination of the Embrittlement Index was performed to study the first case and no sensitivity to this phenomena was found in either material. Nevertheless, an important loss of ductility was shown by both steels in the second case. This was studied by means of the slow strain rate technique with different hydrogen evolutions (produced by different cathodic potentials) at the specimen surface during the test.

    Translated title of the contributionHydrogen embrittlement of API 5LX-52 and X-60 Pipe Line Steels
    Original languageSpanish
    Pages (from-to)331-336
    Number of pages6
    JournalRevista de Metalurgia
    Volume24
    Issue number5
    Publication statusPublished - Sept 1988