Characterization of Inconel 718® superalloy fabricated by wire Arc Additive Manufacturing: effect on mechanical properties and machinability: effect on mechanical properties and machinability

  • ADDILAN Fabricación Aditiva S.L.

Producción científica: Contribución a una revistaArtículorevisión exhaustiva

67 Citas (Scopus)
2 Descargas (Pure)

Resumen

Wire and Arc Additive Manufacturing has the potential to become an appropriate technique to produce large complex-shaped metallic parts. However, a post-processing machining operation is necessary to reach the final geometry. In this work, Inconel 718 walls were manufactured in a monitored environment and their microstructure and mechanical properties were characterised. Then, slot milling operations were performed to investigate the influence of cutting speed and machining direction. The conclusions drawn from this article can be used as a guide for a correct definition of strategies and milling parameters. It was observed that at higher cutting speeds a better surface quality and lower torques are obtained. Moreover, the main novelty of this work is that is shows the influence of the anisotropy of WAAM-Inconel 718 on its machinability. Milling along the torch's travel direction offers better dimensional tolerance values with lower cutting torques, being more favourable than machining in the building direction.
Idioma originalInglés
Páginas (desde-hasta)2665-2676
Número de páginas12
PublicaciónJournal of Materials Research and Technology
Volumen14
DOI
EstadoPublicada - sept 2021

ODS de las Naciones Unidas

Este resultado contribuye a los siguientes Objetivos de Desarrollo Sostenible

  1. ODS 9: Industria, innovación e infraestructura
    ODS 9: Industria, innovación e infraestructura

Palabras clave

  • WAAM
  • Inconel 718
  • Microstructure
  • Machinability
  • Bending moment

Project and Funding Information

  • Funding Info
  • The authors acknowledge the Basque Government for financing the HARIPLUS, HAZITEK 2019 program (ZL-2019/00352) and QUALYFAM project [kk-2020/00042]. The authors are also thankful to the Basque government for supporting the Basque university group on Advanced manufacturing ref: IT1337-19.

Huella

Profundice en los temas de investigación de 'Characterization of Inconel 718® superalloy fabricated by wire Arc Additive Manufacturing: effect on mechanical properties and machinability: effect on mechanical properties and machinability'. En conjunto forman una huella única.

Citar esto