The behavior of API 5LX-52 and X-60 pipe line steels was studied under two hydrogen embrittlement conditions, these were hydrogen embrittlement itself and hydrogen assisted stress cracking. Determination of the Embrittlement Index was performed to study the first case and no sensitivity to this phenomena was found in either material. Nevertheless, an important loss of ductility was shown by both steels in the second case. This was studied by means of the slow strain rate technique with different hydrogen evolutions (produced by different cathodic potentials) at the specimen surface during the test.

Título traducido de la contribuciónHydrogen embrittlement of API 5LX-52 and X-60 Pipe Line Steels
Idioma originalEspañol
Páginas (desde-hasta)331-336
Número de páginas6
PublicaciónRevista de Metalurgia
Volumen24
N.º5
DOI
EstadoPublicada - sept 1988

ODS de las Naciones Unidas

Este resultado contribuye a los siguientes Objetivos de Desarrollo Sostenible

  1. ODS 7: Energía asequible y no contaminante
    ODS 7: Energía asequible y no contaminante

Huella

Profundice en los temas de investigación de 'Fragilizacion por hidrogeno de tubos de acero API 5LX-52 y X-60'. En conjunto forman una huella única.

Citar esto