Resumen
The method comprises placing the powders in an electrically isolating mold, applying a pressure to the powders between 100 and 500MPa and applying to the powders a sintering current at a sintering voltage during a sintering time, for sintering the powders. Before applying the sintering current density, applying an activation current density lower than the sintering current density at an activation voltage greater than the sintering voltage during an activation time lower than the sintering time, to reduce the electrical resistance of the powders.
| Idioma original | Inglés |
|---|---|
| Número de patente | EP3208015 (B1) |
| CIP | B01J19/08||B22F3/087||B22F3/105||B30B11/00||B22F3/16||C22C14/00||C22C21/00||C22C29/08||C22C29/10||C22C32/00 |
| Fecha de prioridad | 19/02/16 |
| Estado | Publicada - 19 feb 2016 |
Huella
Profundice en los temas de investigación de 'Method of sintering electrically conducting powders and an apparatus for carrying out said method'. En conjunto forman una huella única.Citar esto
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver