Resumen
The transformation of vitrified waste, such as bottom ash from municipal waste incineration, into cellular glass-ceramics is convenient, if the additional processing is simple and inexpensive. The present paper aims at presenting a possible route to achieve this goal, based on the recently proposed mechanical foaming of alkali-activated suspensions of waste glass powders, followed by sinter-crystallization at moderate temperatures (from 800 to 900 °C). Compared to previously studied glasses, in this experiment bottom ash-derived glass suspensions underwent progressive hardening at low alkali molarity and in limited times. The firing did not alter the open-celled structure that had developed upon low temperature foaming, owing to a significant crystallization. With an overall porosity of 80%, the optimized foams exhibited a remarkable compressive strength (>6 MPa). Finally, the process had no negative impact on the leaching of toxic elements, which remained well below the thresholds for inert materials.
| Idioma original | Inglés |
|---|---|
| Páginas (desde-hasta) | 133-140 |
| Número de páginas | 8 |
| Publicación | Construction and Building Materials |
| Volumen | 192 |
| DOI | |
| Estado | Publicada - 20 dic 2018 |
| Publicado de forma externa | Sí |
ODS de las Naciones Unidas
Este resultado contribuye a los siguientes Objetivos de Desarrollo Sostenible
-
ODS 11: Ciudades y comunidades sostenibles
-
ODS 12: Producción y consumo responsables
Huella
Profundice en los temas de investigación de 'Up-cycling of vitrified bottom ash from MSWI into glass-ceramic foams by means of ‘inorganic gel casting’ and sinter-crystallization'. En conjunto forman una huella única.Citar esto
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver