Skip to search boxSkip to navigationSkip to main content

High temperature (900 °C) sliding wear of CrNiAlCY coatings deposited by high velocity oxy fuel thermal spray

  • K. Derelizade
    ,
  • ,
  • F. Venturi
    ,
  • R. G. Wellman
    ,
  • A. Kholobystov
    ,
  • T. Hussain(corresponding author)
*Corresponding author for this work
  • University of Nottingham
    ,
  • Rolls-Royce
Research Output:
Contribution to journal
Article
Research
Peer-review

Open access

Abstract

Nickel based superalloy are in demand for high temperature applications and their corrosion, erosion and wear resistance have been investigated for a long time. Nickel chromium (NiCr) alloys are widely used for corrosion resistant coatings, while chromium carbide nickel chromium (CrC-NiCr) alloys are preferred for wear resistant coatings at high temperature. In this study CrNiAlCY coatings were deposited via a liquid fuelled high velocity oxy fuel (HVOF) thermal spray using two spray parameters and tested as wear resistant coatings. Effects of processing parameters on microstructure and mechanical properties of the coatings were investigated. Results showed that higher oxygen flow rates are critical for obtaining coatings with lower porosity and higher microhardness. Coating with lower porosity and higher hardness was chosen for both room temperature (~24 °C) and high temperature (900 °C) unlubricated sliding wear tests in a ball on disc setup. The coating was tested against alumina counterbody under 3 different loading conditions (10, 30 and 60 N). The wear rate of the coating was directly proportional to the applied load at room temperature. In the room temperature tests, wear debris was produced, which then oxidised and pushed away to the edges of the wear track. On the other hand, wear debris was smeared on the wear surface at high temperature tests. The surface was oxidised into Cr2O3 at high temperatures, which acted as a protective layer. Although thermal softening took place at higher temperatures, wear rates under 10 and 30 N were similar to room temperature values due to the protective oxide layer formed on the top surface; however, the oxide layer under 60 N could not withstand the load, started to crack and lost its protective ability.

Research Output Information

Output type

Research Output:
Contribution to journal
Article
Research
Peer-review

Original language

English

Article number

128063

Journal (Volume, Issue Number)

Surface and Coatings Technology (Volume 432)

Publication milestones

  • Published - 25/02/2022

Publication status

Published - 25/02/2022

ISSN

0257-8972

Publication IDs

  • Scopus: 85122510679

Publication metrics

Metrics

SciVal
citations
36
Scopus
citations
SciVal
FWCI
1.82
SciVal
Author count
6
SciVal
Paper percentile
86

PlumX, opens in new tab

Captures
22
Citation count
37