Characterization of Inconel 718® superalloy fabricated by wire Arc Additive Manufacturing: effect on mechanical properties and machinability: effect on mechanical properties and machinability
- Unai Alonso,
- Fernando Veiga,
- ,
- ,
- ,
- ADDILAN Fabricación Aditiva S.L.
Publicación:
Contribución a una revista
Artículo
Investigación
Revisión por expertosAcceso abierto
Abstract
Wire and Arc Additive Manufacturing has the potential to become an appropriate technique to produce large complex-shaped metallic parts. However, a post-processing machining operation is necessary to reach the final geometry.
In this work, Inconel 718 walls were manufactured in a monitored environment and their microstructure and mechanical properties were characterised. Then, slot milling operations were performed to investigate the influence of cutting speed and machining direction. The conclusions drawn from this article can be used as a guide for a correct definition of strategies and milling parameters. It was observed that at higher cutting speeds a better surface quality and lower torques are obtained. Moreover, the main novelty of this work is that is shows the influence of the anisotropy of WAAM-Inconel 718 on its machinability. Milling along the torch's travel direction offers better dimensional tolerance values with lower cutting torques, being more favourable than machining in the building direction.
Research Output Information
Tipo de resultado
Publicación:
Contribución a una revista
Artículo
Investigación
Revisión por expertosIdioma original
InglésPáginas desde-hasta (Número de páginas)
Páginas 2665-2676 (12 páginas)Revista (Volumen, Número de Edición)
Journal of Materials Research and Technology (Volumen 14)Hitos de publicación
- Publicada - 09/2021
Estado de publicación
Publicada - 09/2021
ISSN
2238-7854ID de publicación
- Scopus: 85112507402
Sustainable Development Goals
- ODS 9: Industria, innovación e infraestructura
Publication metrics
Métricas
SciVal
citaciones
73
SciVal
FWCI
2.58
SciVal
Número de autores
4
SciVal
Percentil de artículo
91
SciVal
Percentil superior
10
Descargar estadísticas
Número de descargas
3
PlumX, se abre en una pestaña nueva
Capturas
150
Número de citas
74