Influence of the operating conditions on the behavior and deactivation of a CuO-ZnO-ZrO2@SAPO-11 core-shell-like catalyst in the direct synthesis of DME
- M. Sánchez-Contador,
- A. Ateka(autor correspondiente),
- M. Ibáñez,
- J. Bilbao,
- A. T. Aguayo
Abstract
The behavior of the CuO-ZnO-ZrO2@SAPO-11 core-shell catalyst in the direct synthesis of DME from H2 + CO + CO2 mixtures has been assessed. The effect of the reaction conditions (temperature, pressure, space-time) and feed composition (CO2 and H2 concentration) on the DME yield and selectivity, CO2 and COx (CO2+CO) conversions and stability of the catalyst have been studied. The experiments have been carried out in a fixed-bed reactor in the following condition ranges: 250–325 °C; 10–50 bar; space-time, 1.25–15 g h molC−1; CO2/COx molar ratio in the feed, 0–1; and H2/COx molar ratio in the feed, 2.5–4; time on stream, up to 48 h. Under mild conditions (275–300 °C range, 20–30 bar, space-time over 5 g h molC−1, CO2/COx molar ratio in the 0.5–0.75 range, and H2/COx molar ratio around 3) a good compromise is reached between the yield of DME and the conversion of CO2, with high catalyst stability. Coke deposition is the main cause of catalyst deactivation, formed by condensation of the hydrocarbon byproducts, blocking the metallic sites in the core. The formation rate of this fraction of coke is greater than that of the coke deposited in the SAPO-11 of the shell. Increasing reaction temperature favors the formation of coke, while co-feeding CO2 attenuates this formation, due to the increase of H2O concentration.
Research Output Information
Tipo de resultado
Idioma original
InglésPáginas desde-hasta (Número de páginas)
Páginas 585-597 (13 páginas)Revista (Volumen, Número de Edición)
Renewable Energy (Volumen 138)Hitos de publicación
- Publicada - 08/2019
Estado de publicación
ISSN
0960-1481ID de publicación
- Scopus: 85061324492
Funding Details
Sustainable Development Goals
- ODS 13: Acción por el clima